Graph showing the productivity gain between TIG/GTAW cold wire and TIG/GTAW hot wire in Narrow Groove welding. In hot wire TIG, the greater the thickness of the tube wall, the greater the productivity gain (more than 3 times over thicknesses of 80mm for tube O.D. 355mm in stainless steel)